FABRICANT XINA D'ALTA QUALITAT F51 BRIDA DE COLL DE SOLDADURA D'ACER INOXIDABLE B16.5
Lloc d'origen: | Xina |
Nom de Marca: | Yasco |
Nombre de model: | F51 STAINLESS STEEL WN FLANGE |
Quantitat mínima de comanda: | 1 PEÇA |
preu: | 1USD/PEÇA |
Detalls d'empaquetatge: | EN CAPSA DE FUSTA |
Temps de lliurament: | DIES 3-15 |
Condicions de pagament: | PER TT O LC |
Capacitat de la font: | 300 TONES PER MES |
- DETALLS DEL PRODUCTE
Type: Forged,Welded
Estàndard: ASTM A182, ASME B16.5, EN1092-1, AWWA C206
Capacitat de subministrament: 300 tones per mes
Taller
Different pressure flange, thickness is different, and the bolts they use are different, when pump and valve connect with pipe, the parts of the equipment are also made of the corresponding flange shape, also known as flange connection, usually closured bolted connection parts are also known as flanges, such as the connection of ventilation pipe, this kind of parts can be called "flange type part", but this connection is only part of a device, such as the connection between flange and water pump, it's not inapposite to call water pump as flange type parts, but relative small valve, it can be called as flange type parts.
avantatge competitiu
Why choose the Stainless Steel 304L Flanges of Yasco:
● 24 hours online service -- Anytime, anywhere can provide what you want.
● 100% quality inspection Before Shippment.
● Reasonable and competitive price.
● Best production capability, best quality control, best Service.
ESPECIFICACIONS TÈCNIQUES
Product name: CHINA MANUFACTURER HIGH QUALITY F51 STAINLESS STEEL WELD NECK FLANGE B16.5
Tipus | Forjat, soldat | ||||||||||
Descripció: | Brida de placa Slip on Flange Brida de coll de soldadura Brida d'unió de volta Brida cega Brida de soldadura de socket Brida roscada | ||||||||||
Estàndard: | ASTM A182, ASME B16.5, EN1092-1, Taula D/E, AWWA C206 | ||||||||||
Final | Cara aixecada, cara plana | ||||||||||
Prova: | Test PMI Elongació en 50mm Longitudinal Tractament tèrmic 1050℃ durant 5 min. (WQ) IGC segons ASTM A-262 Practice.E NACE STD: NACE MR0175-MR0103 ED - 2015 Les proves de flaring són ACC. A ASTM A1016 La prova d'aplanament és ACC. A ASTM A1016 DPT als extrems de les canonades Prova de corrents de Foucault Prova per ultrasons Prova de radiografia (raigs X) Prova hidrostàtica | ||||||||||
Embalatge | Caixes de fusta. | ||||||||||
sol·licitud | Transport de petroli i gas, GNL, petroquímica, energia nuclear, construcció naval, pasta i paper, tractament d'aigües residuals, construcció, medicina, alimentació, decoració i altres. | ||||||||||
Temps d'entrega | 20-60 dies després de rebre el dipòsit o 1-10 dies si les mercaderies estan en estoc. | ||||||||||
Terme comercial | EXW, FOB, CIF o com a negociació. | ||||||||||
Termini de pagament | T/T (30% per avançat, 70% contra imatges d'embalatge) o com a negociació. | ||||||||||
Requisit de qualitat | El certificat de prova de molí es proporcionarà amb l'enviament, la inspecció de tercers és acceptable. | ||||||||||
Mercat principal | Europa, sud-est asiàtic, Sud-àfrica, Orient Mitjà, etc. |
Graus disponibles de tub/tub d'acer inoxidable austenític
Grau ASTM | Grau UNS | Grau EN | Grau Comercial estranger | Característiques/Exemples d'aplicació | |
Acer inoxidable austenític | 304 | S30400 | 1.4301 | - | L'acer inoxidable austenític bàsic, per a intercanviador de calor i canonades |
304H | S30409 | 1.4948 | - | Major contingut de carboni, força i resistència a la calor millor que 304 | |
304L | S30403 | 1.4307 | - | Menor contingut de carboni, millor resistència a la corrosió intergranular que 304, millor soldabilitat | |
304LN | S30453 | 1.4311 | - | Menor contingut de carboni amb nitrogen afegit, major resistència. Per a tubs de calor d'aigua d'alimentació. | |
Súper 304 | S30432 | - | Super 304H (NSSMC) | Super 304, tubs de caldera | |
321 | S32100 | 1.4541 | - | Amb contingut de titani, millor resistència a la corrosió que 304 | |
321H | S32109 | 1.4940 | - | Major contingut de carboni, força i resistència a la calor millor que 321 | |
316 | S31600 | 1.4401 | - | Resistència a la corrosió Cl | |
316L | S31603 | 1.4404 | - | Menor contingut de carboni, millor resistència a la corrosió intergranular que 316, millor soldabilitat | |
316LN | S31653 | 1.4406 | - | Menor contingut de carboni amb nitrogen afegit, major resistència. Per a tubs de calor d'aigua d'alimentació. | |
316Ti | S31635 | 1.4571 | - | Amb contingut de titani, millor resistència a la corrosió que 316 | |
316LMoD/316LUG | S31603 | 1.4435 | - | Grau d'urea 316 | |
317L | S31703 | 1.4438 | - | Millor resistència a la corrosió a la picada que 316 | |
317LMN | S31725 | 1.4439 | - | Amb contingut de nitrogen, major resistència i estabilitat de l'estructura | |
310S | S31008 | 1.4845 | - | Alta temperatura i resistència a la corrosió | |
304L | S30403 | 1.4307 | 3RE12 (Sandvik) | Alta puresa d'acer inoxidable de grau HNO3, utilitza 65% HNO3 i inferior | |
310L | S31002 | 1.4335 | 2RE10 (Sandvik) | Alta puresa d'acer inoxidable de grau HNO3, utilitza 85% HNO3 i inferior | |
310H | S31009 | 1.4821 | - | Més contingut de carboni, millor resistència i resistència a la calor que 310 | |
314 | - | 1.4841 | - | Alt contingut de silici, resistència a l'oxidació a alta temperatura i resistència a la ruptura | |
310 MoLN | S31050 | 1.4466 | 2RE69 (Sandvik) | Grau d'urea 310 | |
310HCbN | S31042 | - | HR3C (NSSMC) | Alta resistència, resistència a alta temperatura, tubs de caldera | |
347H | S34709 | 1.4942 | - | Tubs de caldera resistents a l'oxidació i a altes temperatures | |
347HFG | S34710 | - | - | Gran mida 347H, tub de la caldera | |
904L | N08904 | 1.4539 | 2RK65 (Sandvik) | Alt molibdè, té una major resistència a la corrosió | |
Acer inoxidable super austenític | S31254 | S31254 | 1.4547 | 254SMO (Sandvik) | Contingut del 6% de Mo, alta resistència a la corrosió de picats i esquerdes |
N08367 | N08367 | - | AL6XN, AL6XN més (ATI) | ||
N08926 | N08926 | 1.4529 | - | ||
S32652 | S32652 | 1.4652 | 654SMO (Outokumpu) | Contingut del 7% de Mo, millor resistència a la corrosió de picades i esquerdes | |
S31277 | S31277 | - | - |
Composició química del tub/tub d'acer inoxidable austenític
Grau d’acer | C | Mn | P | S | Si | Cr | Ni | Mo | Ti | Nb | Ta | N | V | Cu | Ce | B | Al |
TP304 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-11.0 | - | - | - | - | - | - | - | - | - | - |
TP304L | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-13.0 | - | - | - | - | - | - | - | - | - | - |
TP304H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-11.0 | - | - | - | - | - | - | - | - | - | - |
TP304N | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-11.0 | - | - | - | - | 0.1-0.16 | - | - | - | - | - |
TP304LN | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-12.0 | - | - | - | - | 0.1-0.16 | - | - | - | - | - |
Súper 304 | 0.07-0.13 | 1.0 | 0.04 | 0.01 | 0.3 | 17.0-19.0 | 7.5-10.5 | - | - | 0.3-0.6 | - | 0.05-0.12 | - | 2.5-3.5 | - | 0.001-0.01 | 0.003-0.03 |
TP309S | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 22.0-24.0 | 12.0-15.0 | 0.75 | - | - | - | - | - | - | - | - | - |
TP309H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 22.0-24.0 | 12.0-15.0 | - | - | - | - | - | - | - | - | - | - |
TP310S | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 24.0-26.0 | 19.0-22.0 | 0.75 | - | - | - | - | - | - | - | - | - |
TP310H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 24.0-26.0 | 19.0-22.0 | - | - | - | - | - | - | - | - | - | - |
TP310L | 0.015 | 2.0 | 0.02 | 0.015 | 0.15 | 24.0-26.0 | 19.0-22.0 | 0.1 | - | - | - | 0.1 | - | - | - | - | - |
TP310MoLN | 0.025 | 2.0 | 0.02 | 0.015 | 0.4 | 24.0-26.0 | 20.5-23.5 | 1.6-2.6 | - | - | - | 0.09-0.15 | - | - | - | - | - |
TP310HCbN | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 24.0-26.0 | 19.0-22.0 | 1.6-2.6 | - | - | 0.2-0.6 | 0.15-0.35 | - | - | - | - | - |
1.4841/TP314 | 0.2 | 2.0 | 0.045 | 0.015 | 1.5-2.5 | 24.0-26.0 | 19.0-22.0 | - | - | - | - | 0.11 | - | - | - | - | - |
TP316 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | - | - | - | - | - | - |
TP316L | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | - | - | - | - | - | - |
TP316N | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | 0.1-0.16 | - | - | - | - | - |
TP316H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | - | - | - | - | - | - |
TP316Ti | 0.08 | 2.0 | 0.045 | 0.03 | 0.75 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | 5X(C+N) | - | - | 0.1 | - | - | - | - | - |
TP316LN | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | 0.1-0.16 | - | - | - | - | - |
316LMoD/316LUG | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | - | - | - | - | - | - |
TP317 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 11.0-15.0 | 3.0-4.0 | - | - | - | - | - | - | - | - | - |
TP317L | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 11.0-15.0 | 3.0-4.0 | - | - | - | - | - | - | - | - | - |
TP317LM | 0.03 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 13.5-17.5 | 4.0-5.0 | - | - | - | 0.2 | - | 0.75 | - | - | - |
TP317LMN | 0.03 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-20.0 | 13.5-17.5 | 4.0-5.0 | - | - | - | 0.1-0.2 | - | 0.75 | - | - | - |
TP321 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-12.0 | - | - | - | - | 0.1 | - | - | - | - | - |
TP321H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-12.0 | - | 4(C+N)-0.7 | - | - | - | - | - | - | - | - |
TP347 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-13.0 | - | - | 10*C-0.01 | - | - | - | - | - | - | - |
TP347H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-13.0 | - | - | 8*C-0.01 | - | - | - | - | - | - | - |
347HFG | 0.06-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-13.0 | - | - | 8*C-0.01 | - | - | - | - | - | - | - |
S30815 | 0.05-0.1 | 0.8 | 0.04 | 0.03 | 1.4-2.0 | 20.0-22.0 | 10.0-12.0 | - | - | - | - | 0.14-0.2 | - | - | 0.03-0.08 | - | - |
S31254 | 0.02 | 1.0 | 0.03 | 0.01 | 0.8 | 19.05-20.5 | 17.5-18.5 | 6.0-6.5 | - | - | - | 0.18-0.25 | - | 0.5-1.0 | - | - | - |
904L/N08904 | 0.02 | 2.0 | 0.04 | 0.03 | 1.0 | 19.0-23.0 | 23.0-28.0 | 4.0-5.0 | - | - | - | 0.1 | - | 1.0-2.0 | - | - | - |
N08367 | 0.03 | 2.0 | 0.04 | 0.03 | 1.0 | 20.0-22.0 | 23.5-25.5 | 6.0-7.0 | - | - | - | 0.18-0.25 | - | 0.75 | - | - | - |
N08926 | 0.02 | 2.0 | 0.03 | 0.01 | 0.5 | 19.0-21.0 | 24.0-26.0 | 6.0-7.0 | - | - | - | 0.15-0.25 | - | 0.5-1.0 | - | - | - |
S32654 | - | - | - | - | - | - | - | - | - | - | |||||||
S31277 | - | - | - | - | - | - | - | - | - | - |
Graus disponibles de tubs/tubs d'acer inoxidable dúplex
Grau ASTM | Grau UNS | Grau EN | Grau Comercial estranger | Característiques/Exemples d'aplicació | |
Duplex d'acer inoxidable | S32304 | S32304 | 1.4362 | SAF2304 (Sandvik) | Millor SCC, corrosió per picadura i escletxa, i resistència a la corrosió a l'erosió i alta resistència, la resistència a la fluència és aproximadament 2 vegades superior a 304 i 316. |
S31803 | S31803 | 1.4462 | - | Millor SCC, corrosiu per picadura i escletxa, resistència a la corrosió a l'erosió i alta resistència, menor contingut de Cr i Ni que S32205 | |
S32205 | S32205 | 1.4462 | SAF2205 (Sandvik) | Millor SCC, corrosiu per picadura i escletxa i resistència a la corrosió a l'erosió. | |
Acer inoxidable súper dúplex | S32750 | S32750 | 1.4410 | SAF2507 (Sandvik) | Millor SCC, corrosiu per picadura i escletxa i resistència a la corrosió a l'erosió que l'acer inoxidable dúplex normal, més resistència. |
S31260 | S31260 | - | - | ||
S32550 | S32550 | 1.4507 | UR52+ | ||
S32760 | S32760 | 1.4501 | Zeron100 | ||
S32707 | S32707 | - | - | Hiper dúplex d'acer inoxidable, millor SCC, corrosiu per picadura i escletxa, i resistència a la corrosió a l'erosió que altres acer inoxidable dúplex o acer inoxidable súper dúplex, de major resistència. |
Composició química del tub/tub d'acer inoxidable dúplex
Grau d’acer | C | Mn | P | S | Si | Cr | Ni | Mo | N | Cu | W | Co |
S31200 | 0.03 | 2.0 | 0.045 | 0.03 | 1.0 | 24.0-26.0 | 5.5-6.5 | 1.2-2.0 | 0.14-0.20 | - | - | - |
S31260 | 0.03 | 1.0 | 0.03 | 0.03 | 0.75 | 24.0-26.0 | 5.5-7.5 | 2.5-3.5 | 0.1-0.3 | 0.2-0.8 | 0.1-0.5 | - |
S31500 | 0.03 | 1.2-2.0 | 0.03 | 0.03 | 1.4-2.0 | 18.0-19.0 | 4.3-5.2 | 2.5-3.0 | 0.05-0.1 | - | - | - |
S31803 | 0.03 | 2.0 | 0.03 | 0.02 | 1.0 | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.08-0.2 | - | - | - |
S32001 | 0.03 | 4.0-6.0 | 0.04 | 0.03 | 1.0 | 19.05-21.5 | 1.0-3.0 | 0.6 | 0.05-0.17 | 1.0 | - | - |
S32003 | 0.03 | 1.0 | 0.03 | 0.02 | 1.0 | 19.05-22.5 | 3.0-4.0 | 1.5-2.0 | 0.14-0.20 | - | - | - |
S32101 | 0.04 | 4.0-6.0 | 0.04 | 0.03 | 1.0 | 21.0-22.0 | 1.35-1.7 | 0.1-0.8 | 0.20-0.25 | 0.10-0.8 | - | - |
S32202 | 0.03 | 2.0 | 0.04 | 0.01 | 1.0 | 21.5-24.0 | 1.0-2.8 | 0.45 | 0.18-0.26 | - | - | - |
S32205 | 0.03 | 2.0 | 0.03 | 0.02 | 1.0 | 22.0-23.0 | 4.5-6.5 | 3.0-3.5 | 0.14-0.20 | - | - | - |
S32304 | 0.03 | 2.5 | 0.04 | 0.04 | 1.0 | 21.5-24.5 | 3.0-5.5 | 0.05-0.60 | 0.05-0.20 | 0.05-0.60 | - | - |
S32506 | 0.03 | 1.0 | 0.04 | 0.015 | 0.9 | 24.0-26.0 | 5.5-7.2 | 3.0-3.5 | 0.08-0.2 | - | 0.05-0.3 | - |
S32520 | 0.03 | 1.5 | 0.035 | 0.02 | 0.8 | 23.0-25.0 | 5.5-8.0 | 3.0-5.0 | 0.20-0.35 | 0.50-3.0 | - | - |
S32550 | 0.04 | 1.5 | 0.04 | 0.03 | 1.0 | 24.0-27.0 | 4.5-6.5 | 2.9-3.9 | 0.10-0.25 | 1.5-2.5 | - | 0.5-2.0 |
S32707 | 0.03 | 1.5 | 0.035 | 0.01 | 0.5 | 26.0-29.0 | 5.5-9.5 | 4.0-5.0 | 0.3-0.5 | 1.0 | - | - |
S32750 | 0.03 | 1.2-2.0 | 0.035 | 0.02 | 0.8 | 24.0-26.0 | 6.0-8.0 | 3.0-5.0 | 0.24-0.32 | 0.5 | - | - |
S32760 | 0.03 | 1.0 | 0.03 | 0.01 | 1.0 | 24.0-26.0 | 6.0-8.0 | 3.0-4.0 | 0.20-0.30 | 0.5-1.0 | 0.05-1.0 | - |
S32906 | 0.03 | 0.8-1.5 | 0.03 | 0.03 | 0.8 | 28.0-30.0 | 5.8-7.5 | 1.50-2.60 | 0.30-0.40 | 0.8 | - | - |
Graus disponibles de tubs/tubs d'acer inoxidable ferrític i martensític
Grau ASTM | Grau UNS | Grau EN | Grau Comercial estranger | Característiques/Exemples d'aplicació | ||
Acer inoxidable ferrític | 405 | S40500 | 1.4002 | - | Resistència a altes temperatures, resistència a l'oxidació i resistència a la corrosió, tub d'intercanviador de calor d'aire. | S'utilitza a una temperatura de 700 °C |
- | - | 1.4724 | SIC9(Sanyo)/1C256(Sandvik) | S'utilitza a una temperatura de 850 °C | ||
430 | S43000 | 1.4016 | - | S'utilitza a una temperatura de 800 °C | ||
- | - | 1.4742 | SIC10(Sanyo)/1C356(Sandvik) | S'utilitza a una temperatura de 1000 °C | ||
- | - | 1.4762 | SIC12 (Sanyo) | S'utilitza a una temperatura de 1150 °C | ||
- | - | - | QS25T (Sanyo) | S'utilitza a una temperatura de 1100 °C | ||
TP446-1/TP446-2 | S44600 | 1.4749 | 2C52/2C48 (Sandvik) | Corrosió d'oxidació a alta temperatura a l'aire, bona resistència a la reducció de gasos sulfurosos, resistència a Cu, Al i Zn fosos, tubs d'intercanviador de calor d'aire. | S'utilitza a una temperatura de 1000 °C per a 446-1 i 1075 °C per a 446-2 | |
439 | S43035 | 1.4510 | - | Bona resistència a la corrosió SCC, tub intercanviador de calor. | ||
444 | S44400 | 1.4521 | - | |||
Acer inoxidable súper ferrític | S44660 | S44660 | - | Sea-Cure (tub Plymouth) | Bona resistència a la corrosió de clorurs i esquerdes, immune a SCC, bona resistència a l'erosió, alta conductivitat tèrmica i baixa expansió tèrmica Dessalinització, tubs de condensació d'aigua de mar elèctrica. | |
S44735 | S44735 | - | AL29-4C (ATI) | |||
S44736 | S44736 | - | AL29-4-2 (ATI) | |||
Acer inoxidable martensític | 410S | S41008 | 1.4000 | - | Baixa resistència a la corrosió, baixa expansió tèrmica, tubs d'intercanviador de calor. | |
410 | S41000 | 1.4006 | - | |||
420 | S42000 | 1.4021 | API/13Cr 180 | Endurit per tractament tèrmic, alta duresa. | ||
420J2 | S42000 | 1.4028 | - | |||
431 | S43100 | - | - | |||
17-4 hores | S17400 | 1.4542 | - | Acer inoxidable martensític d'enduriment per precipitació, alta resistència. | ||
Acer inoxidable súper martensític | 13Cr110 | S41426 | 1.4313 | SM13CRS (NSSMC) | Alta resistència, bona resistència a la corrosió, oli API i tub o acoblament de la carcassa. | |
- | - | 1.4418 | - | |||
17Cr110/125 | - | - | SM17CRS (NSSMC) |
Composició química del tub/tub d'acer inoxidable ferrític i martensític
Estàndard | Grau d’acer | C | Mn | P | S | Si | Cr | Ni | Mo | N | Nb | Ti | Al | Cu |
A/SA268 | TP405 | ≤ 0.08 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 11.5-14.5 | ≤ 0.50 | - | - | - | - | 0.1-0.3 | - |
A/SA268 | TP410 | ≤ 0.15 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 11.5-13.5 | - | - | - | - | - | - | - |
A/SA268 | TP410S | ≤ 0.08 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 11.5-14.5 | - | - | - | - | - | - | - |
A/SA268 | TP430 | ≤ 0.12 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 16.00-18.00 | - | - | - | - | - | - | - |
A/SA268 | TP430Ti | ≤ 0.10 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 16.00-19.5 | ≤ 0.75 | - | - | - | 5C-0.75 | - | - |
A/SA268 | TP446-1 | ≤ 0.20 | ≤ 1.50 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 23.00-27.00 | ≤ 0.75 | - | 0.25 | - | - | - | - |
A/SA268 | TP446-2 | ≤ 0.12 | ≤ 1.50 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 23.00-27.00 | ≤ 0.50 | - | 0.25 | - | - | - | - |
A/SA268 | TP409 | ≤ 0.08 | ≤ 1.00 | ≤ 0.045 | ≤ 0.030 | ≤ 1.00 | 10.50-11.70 | ≤ 0.50 | - | - | - | 6C-0.75 | - | - |
A/SA268 | TP439 | ≤ 0.07 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 17.00-19.00 | ≤ 0.50 | - | 0.04 | - | 0.2+4(C+N)-1.1 | - | - |
A/SA268 | TP444 | ≤ 0.025 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 17.50-19.50 | ≤ 1.00 | 1.75-2.5 | 0.035 | - | (Ti+Cb): 0.2+4(C+N)~0.8 | - | - |
A/SA756/268 | 440C | 0.95-1.10 | ≤ 1.00 | ≤ 0.025 | ≤ 0.025 | ≤ 1.00 | 16.00-18.00 | - | 0.4-0.7 | - | - | - | - | - |
A/SA693 | 17-4 hores | ≤ 0.07 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 15.50-17.50 | 3.0-5.0 | - | - | 0.15-0.45 | - | - | 3.0-5.0 |
GOST9941-81 | 15Cr25Ti | ≤ 0.15 | ≤ 0.80 | ≤ 0.035 | ≤ 0.025 | ≤ 1.00 | 24.00-27.00 | - | - | - | - | 5C-0.90 | - | - |
API 5CT | L80/9Cr | ≤ 0.15 | 0.30-0.60 | ≤ 0.020 | ≤ 0.010 | ≤ 1.00 | 8.00-10.00 | - | 0.9-1.1 | - | - | - | - | - |
API 5CT | L80/13Cr | 0.15-0.22 | 0.25-1.00 | ≤ 0.020 | ≤ 0.010 | ≤ 1.00 | 12.0-14.0 | - | - | - | - | - | - | - |
EN10088-1 | 1.4724 | ≤ 0.12 | ≤ 1.00 | ≤ 0.040 | ≤ 0.015 | 0.70-1.40 | 12.0-14.0 | - | - | - | - | - | 0.7-1.2 | - |
EN10088-1 | 1.4742 | ≤ 0.12 | ≤ 1.00 | ≤ 0.040 | ≤ 0.015 | 0.70-1.40 | 17.0-19.0 | - | - | - | - | - | 0.7-1.2 | - |
EN10088-1 | 1.4762 | ≤ 0.12 | ≤ 1.00 | ≤ 0.040 | ≤ 0.015 | 0.70-1.40 | 23.0-26.0 | - | - | - | - | - | 1.2-1.7 | - |
A/SA268 | S44660 | ≤ 0.030 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 25.0-28.0 | - | 3.0-4.0 | 0.04 | - | (Ti+Cb)=0.2~1.0 i ≥6(C+N)~0.8 | - | - |
A/SA268 | S44735 | ≤ 0.030 | ≤ 1.00 | ≤ 0.040 | ≤ 0.030 | ≤ 1.00 | 28.0-30.0 | ≤ 1.00 | 3.6-4.2 | 0.045 | - | (Ti+Cb)=0.2~1.0 i ≥6(C+N)~0.8 | - | - |