Contact Us
Email : [email protected]
Phone : 0086 731 85240616
Add : Room 2702, Building #2, Zhongyijiujun, No.29, South Junxing Road, Yuelu District, Changsha, Hunan, China.
CHINA FACTORY BEST QUALITY SS316L SHORT TYPE STAINLESS PIPE COLLAR LAP JOINT MSS SP-43
Inquiry Now- PRODUCT DETAILS
Type: Forged
Connection: Butt-welded
Standard: ASTM A403,ASME B16.9,MSS SP-43
Specification: Long type,Short type
Surface: Pickled,Polishing and mirror.
Supply ability: 300ton per month
Workshop
Stainless steel stub end is a forming process that stretches or compresses the outer edge of the work piece to produce a vertical edge with a small height. Divided into convex curve flange and concave curve flange.
Packing and Loading
In the process of transportation, in order to ensure the safety of product transportation, we use wooden cases, iron frame, plastic bags and other wooden pallets, or according to customer's requirement.
TECHNICAL SPECIFICATION
Product name: CHINA FACTORY BEST QUALITY SS316L SHORT TYPE STAINLESS PIPE COLLAR LAP JOINT MSS SP-43
Type | Forged | ||||||||||
Size | NPS 1/8"- 48" SCH: 5S,10/10S/,20,30,STD,40/40S,60,80/80S,XS,100,120,140,160,XXS OD: 0.04"- 72" (1.0mm-1828.80mm) WT: 0.004"- 2" (0.1mm-50.8mm) | ||||||||||
Specification | Long Type,Short Type as per ASTM A403,ASME B16.9,MSS SP-43 | ||||||||||
End | Plain end,Beveled end,Threaded end. | ||||||||||
Surface /Finish | Pickled,Mechanically Polished,Bright Annealed,Electro Polished | ||||||||||
Test: | PMI Test Elongation in 50mm Longitudinal Heat Treatment 1050℃ for 5Min. (W.Q) IGC as per ASTM A-262 Practice.E NACE STD: NACE MR0175-MR0103 ED - 2015 Flaring Testing is ACC. TO ASTM A1016 Flattening Testing is ACC. TO ASTM A1016 DPT on pipe ends Eddy Current Test Ultrasonic Test Radiography Test (X-ray) Hydrostatic Test | ||||||||||
Packing | Wooden boxes. | ||||||||||
Application | Oil & Gas transportation,LNG,petrochemical,nuclear power,shipbuilding,pulp and paper,sewage treatment,construction,medicine,foodstuffs,decoration and others. | ||||||||||
Delivery time | 20-60 days after receiving the deposit or 1-10 days if goods in stock. | ||||||||||
Trade term | EXW,FOB,CIF or as negotiation. | ||||||||||
Payment term | T/T(30% in advance,70% against packing pictures) or as negotiation. | ||||||||||
Quality requirement | Mill Test Certificated will be provided with shipment,Third Party Inspection is acceptable. | ||||||||||
Main Market | Europe,Southeast Asia,South Africa,Middle East etc. |
Available Grades of Austenitic stainless steel tube/Pipe
ASTM Grade | UNS Grade | EN Grade | Foreign Commercial Grade | Characteristics/Examples of Application | |
Austenitic Stainless Steel | 304 | S30400 | 1.4301 | - | The basic austenitic stainless steel,for heat exchanger and piping |
304H | S30409 | 1.4948 | - | Higher carbon content,strength and heat resistance better than 304 | |
304L | S30403 | 1.4307 | - | Lower carbon content,better resistance to intergranular corrosion than 304,better weldability | |
304LN | S30453 | 1.4311 | - | Lower carbon content with Nitrogen added,higher strength.For feed water heat tubes. | |
Super 304 | S30432 | - | Super 304H(NSSMC) | Super 304,boiler tubes | |
321 | S32100 | 1.4541 | - | With content of Titanium,better corrosive resistance than 304 | |
321H | S32109 | 1.4940 | - | Higher carbon content,strength and heat resistance better than 321 | |
316 | S31600 | 1.4401 | - | Cl-corrosive resistance | |
316L | S31603 | 1.4404 | - | Lower carbon content,better resistance to intergranular corrosion than 316,better weldability | |
316LN | S31653 | 1.4406 | - | Lower carbon content with Nitrogen added,higher strength.For feed water heat tubes. | |
316Ti | S31635 | 1.4571 | - | With content of Titanium,better corrosive resistance than 316 | |
316LMoD/316LUG | S31603 | 1.4435 | - | Urea Grade 316 | |
317L | S31703 | 1.4438 | - | Better pitting corrosive resistance than 316 | |
317LMN | S31725 | 1.4439 | - | With content of Nitrogen,higher strength and structure stability | |
310S | S31008 | 1.4845 | - | High termprature and corrosive resistance | |
304L | S30403 | 1.4307 | 3RE12(Sandvik) | High purity of HNO3 grade stainless steel,utilized 65% HNO3 and lower | |
310L | S31002 | 1.4335 | 2RE10(Sandvik) | High purity of HNO3 grade stainless steel,utilized 85% HNO3 and lower | |
310H | S31009 | 1.4821 | - | Higer carbon content,better strength and heat resistance than 310 | |
314 | - | 1.4841 | - | High Silicon content,high temperature oxidation resistance and creep-rupture strength | |
310MoLN | S31050 | 1.4466 | 2RE69(Sandvik) | Urea Grade 310 | |
310HCbN | S31042 | - | HR3C(NSSMC) | High strength,high temperature resistance,boiler tubes | |
347H | S34709 | 1.4942 | - | Oxidation resistant and high temperature resistance boiler tubes | |
347HFG | S34710 | - | - | High grain size 347H,boiler tube | |
904L | N08904 | 1.4539 | 2RK65(Sandvik) | High Molybdenum,it has higher corrosion resistance | |
Super Austenitic Stainless Steel | S31254 | S31254 | 1.4547 | 254SMO(Sandvik) | 6% Mo content,high pitting and crevice corrosion resistance |
N08367 | N08367 | - | AL6XN,AL6XN plus(ATI) | ||
N08926 | N08926 | 1.4529 | - | ||
S32652 | S32652 | 1.4652 | 654SMO(Outokumpu) | 7% Mo content,better pitting and crevice corrosion resistance | |
S31277 | S31277 | - | - |
Chemical Composition of Austenitic stainless steel pipe/Tube
Steel Grade | C | Mn | P | S | Si | Cr | Ni | Mo | Ti | Nb | Ta | N | V | Cu | Ce | B | Al |
TP304 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-11.0 | - | - | - | - | - | - | - | - | - | - |
TP304L | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-13.0 | - | - | - | - | - | - | - | - | - | - |
TP304H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-11.0 | - | - | - | - | - | - | - | - | - | - |
TP304N | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-11.0 | - | - | - | - | 0.1-0.16 | - | - | - | - | - |
TP304LN | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 8.0-12.0 | - | - | - | - | 0.1-0.16 | - | - | - | - | - |
Super 304 | 0.07-0.13 | 1.0 | 0.04 | 0.01 | 0.3 | 17.0-19.0 | 7.5-10.5 | - | - | 0.3-0.6 | - | 0.05-0.12 | - | 2.5-3.5 | - | 0.001-0.01 | 0.003-0.03 |
TP309S | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 22.0-24.0 | 12.0-15.0 | 0.75 | - | - | - | - | - | - | - | - | - |
TP309H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 22.0-24.0 | 12.0-15.0 | - | - | - | - | - | - | - | - | - | - |
TP310S | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 24.0-26.0 | 19.0-22.0 | 0.75 | - | - | - | - | - | - | - | - | - |
TP310H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 24.0-26.0 | 19.0-22.0 | - | - | - | - | - | - | - | - | - | - |
TP310L | 0.015 | 2.0 | 0.02 | 0.015 | 0.15 | 24.0-26.0 | 19.0-22.0 | 0.1 | - | - | - | 0.1 | - | - | - | - | - |
TP310MoLN | 0.025 | 2.0 | 0.02 | 0.015 | 0.4 | 24.0-26.0 | 20.5-23.5 | 1.6-2.6 | - | - | - | 0.09-0.15 | - | - | - | - | - |
TP310HCbN | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 24.0-26.0 | 19.0-22.0 | 1.6-2.6 | - | - | 0.2-0.6 | 0.15-0.35 | - | - | - | - | - |
1.4841/TP314 | 0.2 | 2.0 | 0.045 | 0.015 | 1.5-2.5 | 24.0-26.0 | 19.0-22.0 | - | - | - | - | 0.11 | - | - | - | - | - |
TP316 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | - | - | - | - | - | - |
TP316L | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | - | - | - | - | - | - |
TP316N | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | 0.1-0.16 | - | - | - | - | - |
TP316H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | - | - | - | - | - | - |
TP316Ti | 0.08 | 2.0 | 0.045 | 0.03 | 0.75 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | 5X(C+N) | - | - | 0.1 | - | - | - | - | - |
TP316LN | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | 0.1-0.16 | - | - | - | - | - |
316LMoD/316LUG | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 16.0-18.0 | 10.0-14.0 | 2.0-3.0 | - | - | - | - | - | - | - | - | - |
TP317 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 11.0-15.0 | 3.0-4.0 | - | - | - | - | - | - | - | - | - |
TP317L | 0.035 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 11.0-15.0 | 3.0-4.0 | - | - | - | - | - | - | - | - | - |
TP317LM | 0.03 | 2.0 | 0.045 | 0.03 | 1.0 | 18.0-20.0 | 13.5-17.5 | 4.0-5.0 | - | - | - | 0.2 | - | 0.75 | - | - | - |
TP317LMN | 0.03 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-20.0 | 13.5-17.5 | 4.0-5.0 | - | - | - | 0.1-0.2 | - | 0.75 | - | - | - |
TP321 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-12.0 | - | - | - | - | 0.1 | - | - | - | - | - |
TP321H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-12.0 | - | 4(C+N)-0.7 | - | - | - | - | - | - | - | - |
TP347 | 0.08 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-13.0 | - | - | 10*C-0.01 | - | - | - | - | - | - | - |
TP347H | 0.04-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-13.0 | - | - | 8*C-0.01 | - | - | - | - | - | - | - |
347HFG | 0.06-0.1 | 2.0 | 0.045 | 0.03 | 1.0 | 17.0-19.0 | 9.0-13.0 | - | - | 8*C-0.01 | - | - | - | - | - | - | - |
S30815 | 0.05-0.1 | 0.8 | 0.04 | 0.03 | 1.4-2.0 | 20.0-22.0 | 10.0-12.0 | - | - | - | - | 0.14-0.2 | - | - | 0.03-0.08 | - | - |
S31254 | 0.02 | 1.0 | 0.03 | 0.01 | 0.8 | 19.05-20.5 | 17.5-18.5 | 6.0-6.5 | - | - | - | 0.18-0.25 | - | 0.5-1.0 | - | - | - |
904L/N08904 | 0.02 | 2.0 | 0.04 | 0.03 | 1.0 | 19.0-23.0 | 23.0-28.0 | 4.0-5.0 | - | - | - | 0.1 | - | 1.0-2.0 | - | - | - |
N08367 | 0.03 | 2.0 | 0.04 | 0.03 | 1.0 | 20.0-22.0 | 23.5-25.5 | 6.0-7.0 | - | - | - | 0.18-0.25 | - | 0.75 | - | - | - |
N08926 | 0.02 | 2.0 | 0.03 | 0.01 | 0.5 | 19.0-21.0 | 24.0-26.0 | 6.0-7.0 | - | - | - | 0.15-0.25 | - | 0.5-1.0 | - | - | - |
S32654 | - | - | - | - | - | - | - | - | - | - | |||||||
S31277 | - | - | - | - | - | - | - | - | - | - |
Available Grades of Duplex Stainless Steel Tube/Pipe
ASTM Grade | UNS Grade | EN Grade | Foreign Commercial Grade | Characteristics/Examples of Application | |
Duplex Stainless Steel | S32304 | S32304 | 1.4362 | SAF2304(Sandvik) | Better SCC,pitting and crevice corrosive,and erosion corrosive resistance and high strength,yield strength is about 2 times higher than 304 and 316. |
S31803 | S31803 | 1.4462 | - | Better SCC,pitting and crevice corrosive,and erosion corrosive resistance and high strength,lower Cr and Ni content than S32205 | |
S32205 | S32205 | 1.4462 | SAF2205(Sandvik) | Better SCC,pitting and crevice corrosive,and erosion corrosive resistance. | |
Super Duplex Stainless Steel | S32750 | S32750 | 1.4410 | SAF2507(Sandvik) | Better SCC,pitting and crevice corrosive,and erosion corrosive resistance than ordinary duplex stainless steel,higher strength. |
S31260 | S31260 | - | - | ||
S32550 | S32550 | 1.4507 | UR52+ | ||
S32760 | S32760 | 1.4501 | Zeron100 | ||
S32707 | S32707 | - | - | Hyper duplex stainless steel,better SCC,pitting and crevice corrosive,and erosion corrosive resistance than other duplex stainless steel or super duplex stainless steel,higher strength. |
Chemical Composition of Duplex Stainless Steel Pipe/Tube
Steel Grade | C | Mn | P | S | Si | Cr | Ni | Mo | N | Cu | W | Co |
S31200 | 0.03 | 2.0 | 0.045 | 0.03 | 1.0 | 24.0-26.0 | 5.5-6.5 | 1.2-2.0 | 0.14-0.20 | - | - | - |
S31260 | 0.03 | 1.0 | 0.03 | 0.03 | 0.75 | 24.0-26.0 | 5.5-7.5 | 2.5-3.5 | 0.1-0.3 | 0.2-0.8 | 0.1-0.5 | - |
S31500 | 0.03 | 1.2-2.0 | 0.03 | 0.03 | 1.4-2.0 | 18.0-19.0 | 4.3-5.2 | 2.5-3.0 | 0.05-0.1 | - | - | - |
S31803 | 0.03 | 2.0 | 0.03 | 0.02 | 1.0 | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.08-0.2 | - | - | - |
S32001 | 0.03 | 4.0-6.0 | 0.04 | 0.03 | 1.0 | 19.05-21.5 | 1.0-3.0 | 0.6 | 0.05-0.17 | 1.0 | - | - |
S32003 | 0.03 | 1.0 | 0.03 | 0.02 | 1.0 | 19.05-22.5 | 3.0-4.0 | 1.5-2.0 | 0.14-0.20 | - | - | - |
S32101 | 0.04 | 4.0-6.0 | 0.04 | 0.03 | 1.0 | 21.0-22.0 | 1.35-1.7 | 0.1-0.8 | 0.20-0.25 | 0.10-0.8 | - | - |
S32202 | 0.03 | 2.0 | 0.04 | 0.01 | 1.0 | 21.5-24.0 | 1.0-2.8 | 0.45 | 0.18-0.26 | - | - | - |
S32205 | 0.03 | 2.0 | 0.03 | 0.02 | 1.0 | 22.0-23.0 | 4.5-6.5 | 3.0-3.5 | 0.14-0.20 | - | - | - |
S32304 | 0.03 | 2.5 | 0.04 | 0.04 | 1.0 | 21.5-24.5 | 3.0-5.5 | 0.05-0.60 | 0.05-0.20 | 0.05-0.60 | - | - |
S32506 | 0.03 | 1.0 | 0.04 | 0.015 | 0.9 | 24.0-26.0 | 5.5-7.2 | 3.0-3.5 | 0.08-0.2 | - | 0.05-0.3 | - |
S32520 | 0.03 | 1.5 | 0.035 | 0.02 | 0.8 | 23.0-25.0 | 5.5-8.0 | 3.0-5.0 | 0.20-0.35 | 0.50-3.0 | - | - |
S32550 | 0.04 | 1.5 | 0.04 | 0.03 | 1.0 | 24.0-27.0 | 4.5-6.5 | 2.9-3.9 | 0.10-0.25 | 1.5-2.5 | - | 0.5-2.0 |
S32707 | 0.03 | 1.5 | 0.035 | 0.01 | 0.5 | 26.0-29.0 | 5.5-9.5 | 4.0-5.0 | 0.3-0.5 | 1.0 | - | - |
S32750 | 0.03 | 1.2-2.0 | 0.035 | 0.02 | 0.8 | 24.0-26.0 | 6.0-8.0 | 3.0-5.0 | 0.24-0.32 | 0.5 | - | - |
S32760 | 0.03 | 1.0 | 0.03 | 0.01 | 1.0 | 24.0-26.0 | 6.0-8.0 | 3.0-4.0 | 0.20-0.30 | 0.5-1.0 | 0.05-1.0 | - |
S32906 | 0.03 | 0.8-1.5 | 0.03 | 0.03 | 0.8 | 28.0-30.0 | 5.8-7.5 | 1.50-2.60 | 0.30-0.40 | 0.8 | - | - |
Available Grades of Ferritic and Martensitic Stainless Steel Tube/Pipe
ASTM Grade | UNS Grade | EN Grade | Foreign Commercial Grade | Characteristics/Examples of Application | ||
Ferritic Stainless Steel | 405 | S40500 | 1.4002 | - | High temperature resistance,oxidation resistance,and corrosion resistance,air heat exchanger tube. | Utilized at temperature 700°C |
- | - | 1.4724 | SIC9(Sanyo)/1C256(Sandvik) | Utilized at temperature 850°C | ||
430 | S43000 | 1.4016 | - | Utilized at temperature 800°C | ||
- | - | 1.4742 | SIC10(Sanyo)/1C356(Sandvik) | Utilized at temperature 1000°C | ||
- | - | 1.4762 | SIC12(Sanyo) | Utilized at temperature 1150°C | ||
- | - | - | QS25T(Sanyo) | Utilized at temperature 1100°C | ||
TP446-1/TP446-2 | S44600 | 1.4749 | 2C52/2C48(Sandvik) | High temperature oxidation corrosion in air,good resistance to reducing sulphurous gases,resistance to molten Cu,Al and Zn,air heat exchanger tubes. | Utilized at temperature 1000°C for 446-1 and 1075°C for 446-2 | |
439 | S43035 | 1.4510 | - | Good resistance to SCC corrosion,heat exchanger tube. | ||
444 | S44400 | 1.4521 | - | |||
Super Ferritic Stainless Steel | S44660 | S44660 | - | Sea-Cure(Plymouth Tube) | Good resistance to chloride pitting and crevice corrosion,immune to SCC,good erosion resistance,high thermal conductivity and low thermal expansion Desalination,power sea-water condenser tubes. | |
S44735 | S44735 | - | AL29-4C(ATI) | |||
S44736 | S44736 | - | AL29-4-2(ATI) | |||
Martensitic Stainless Steel | 410S | S41008 | 1.4000 | - | Low corrosion resistance,low thermal expansion,heat exchanger tubes. | |
410 | S41000 | 1.4006 | - | |||
420 | S42000 | 1.4021 | API/13Cr 180 | Hardened by heat treatment,high hardness. | ||
420J2 | S42000 | 1.4028 | - | |||
431 | S43100 | - | - | |||
17-4PH | S17400 | 1.4542 | - | Precipitation hardening martensitic stainless steel,high strength. | ||
Super Martensitic Stainless Steel | 13Cr110 | S41426 | 1.4313 | SM13CRS(NSSMC) | High strength,good corrosive resistance,API oil and casing pipe or coupling. | |
- | - | 1.4418 | - | |||
17Cr110/125 | - | - | SM17CRS(NSSMC) |
Chemical Composition of Ferritic and Martensitic Stainless Steel Pipe/Tube
Standard | Steel Grade | C | Mn | P | S | Si | Cr | Ni | Mo | N | Nb | Ti | Al | Cu |
A/SA268 | TP405 | ≤0.08 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 11.5-14.5 | ≤0.50 | - | - | - | - | 0.1-0.3 | - |
A/SA268 | TP410 | ≤0.15 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 11.5-13.5 | - | - | - | - | - | - | - |
A/SA268 | TP410S | ≤0.08 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 11.5-14.5 | - | - | - | - | - | - | - |
A/SA268 | TP430 | ≤0.12 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 16.00-18.00 | - | - | - | - | - | - | - |
A/SA268 | TP430Ti | ≤0.10 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 16.00-19.5 | ≤0.75 | - | - | - | 5C-0.75 | - | - |
A/SA268 | TP446-1 | ≤0.20 | ≤1.50 | ≤0.040 | ≤0.030 | ≤1.00 | 23.00-27.00 | ≤0.75 | - | 0.25 | - | - | - | - |
A/SA268 | TP446-2 | ≤0.12 | ≤1.50 | ≤0.040 | ≤0.030 | ≤1.00 | 23.00-27.00 | ≤0.50 | - | 0.25 | - | - | - | - |
A/SA268 | TP409 | ≤0.08 | ≤1.00 | ≤0.045 | ≤0.030 | ≤1.00 | 10.50-11.70 | ≤0.50 | - | - | - | 6C-0.75 | - | - |
A/SA268 | TP439 | ≤0.07 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 17.00-19.00 | ≤0.50 | - | 0.04 | - | 0.2+4(C+N)-1.1 | - | - |
A/SA268 | TP444 | ≤0.025 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 17.50-19.50 | ≤1.00 | 1.75-2.5 | 0.035 | - | (Ti+Cb):0.2+4(C+N)~0.8 | - | - |
A/SA756/268 | 440C | 0.95-1.10 | ≤1.00 | ≤0.025 | ≤0.025 | ≤1.00 | 16.00-18.00 | - | 0.4-0.7 | - | - | - | - | - |
A/SA693 | 17-4PH | ≤0.07 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 15.50-17.50 | 3.0-5.0 | - | - | 0.15-0.45 | - | - | 3.0-5.0 |
GOST9941-81 | 15Cr25Ti | ≤0.15 | ≤0.80 | ≤0.035 | ≤0.025 | ≤1.00 | 24.00-27.00 | - | - | - | - | 5C-0.90 | - | - |
API 5CT | L80/9Cr | ≤0.15 | 0.30-0.60 | ≤0.020 | ≤0.010 | ≤1.00 | 8.00-10.00 | - | 0.9-1.1 | - | - | - | - | - |
API 5CT | L80/13Cr | 0.15-0.22 | 0.25-1.00 | ≤0.020 | ≤0.010 | ≤1.00 | 12.0-14.0 | - | - | - | - | - | - | - |
EN10088-1 | 1.4724 | ≤0.12 | ≤1.00 | ≤0.040 | ≤0.015 | 0.70-1.40 | 12.0-14.0 | - | - | - | - | - | 0.7-1.2 | - |
EN10088-1 | 1.4742 | ≤0.12 | ≤1.00 | ≤0.040 | ≤0.015 | 0.70-1.40 | 17.0-19.0 | - | - | - | - | - | 0.7-1.2 | - |
EN10088-1 | 1.4762 | ≤0.12 | ≤1.00 | ≤0.040 | ≤0.015 | 0.70-1.40 | 23.0-26.0 | - | - | - | - | - | 1.2-1.7 | - |
A/SA268 | S44660 | ≤0.030 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 25.0-28.0 | - | 3.0-4.0 | 0.04 | - | (Ti+Cb)=0.2~1.0 & ≥6(C+N)~0.8 | - | - |
A/SA268 | S44735 | ≤0.030 | ≤1.00 | ≤0.040 | ≤0.030 | ≤1.00 | 28.0-30.0 | ≤1.00 | 3.6-4.2 | 0.045 | - | (Ti+Cb)=0.2~1.0 & ≥6(C+N)~0.8 | - | - |